High Heat Gloves
234-AKV-ZP
234-AZ-Z
234-AKV-KV
234-ZP
Combo glove. 19
oz. aluminized Kevlar®-aramid fiber blend on back for
up to 2000° F radiant protection. 35 oz. Zetex Plus® palm
for short duration up to 2000° F. Moderate abrasion resistance.
Combo glove, 35 oz. Zetex®
glass on palm for short durations up to 1000° F. 25 oz.,
aluminized Zetex® for up to 2000° F radiant
protection on back side. Moderate to poor abrasion
resistance.
Combo glove, 19 oz. aluminized
Kevlar® -aramid blend on back for near 2000° F
radiant protection. 22 oz. Kevlar - aramid blend palm for
working temperature of 400 F-600 F and good abrasion resistance.
35 oz. Zetex Plus®
treated fiberglass. Short duration up to 2000° F.
Moderate abrasion resistance. Double layer gloves are
recommended when working with higher heats.
234-V
234-GL
234-KTW
234-KT
36 oz. Vertex™ vermiculite
coated fiberglass. Short durations up to 2000° F.
Moderate abrasion resistance. Shown with steel mesh
reinforcemtn for better abrasion resistance
26 oz. white generic glass
fabric. Short durations up to 1000° F. Poor abrasion
resistance.
8 oz. Kevlar®
twill. Working temperature of approximately 500° - 600° F.
Superior abrasion resistance. Good dexterity.
22 oz. Kevlar®
terry. Working temperature of approximately 600° F.
Superior abrasion resistance.
234-PBI
234-MT
234-THL
234-AKV
Polybenzamidazole blend available
in 22 oz. or 45 oz. Higher working temperatures near
fiberglass levels with superior abrasion resistance.
45 oz. PBI offers a thick barrier for longer heat duration
but less dexterity.
Terry cotton "mock twist" glove
for lower temperatures. Can be used as a baker's glove.
Brown thermal leather withstands
premature hardening up to 500° F. Good abrasion
resistance.
19 oz. aluminized Kevlar®
-aramid fiber blend. Up to 2000° F radiant heat.
Some sparks and molten splash. Good abrasion resistance.
234-AZ
234-ARH
234-Z
25
oz. aluminized Zetex®.
Up to 2000° F radiant heat. Some spark and splash.
Moderate abrasion resistance.
19 oz. aluminized rayon. Up
to 2000° F radiant heat. Some sparks and molten splash.
Moderate abrasion resistance.
35 oz. Zetex® fiberglass.
Sort durations up to 1000° F. Moderate to poor abrasion
resistance.